video
Tube For Perforating Gun
Tube For Perforating Gun
1/2
<< /span>
>

Tubes are the main raw material for the manufacture of high-performance perforating guns for oil and gas wells.

 

 





Delivery Time: 7-25 Days after Receiving the Deposit.

 

Tube for Perforating Gun

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

Tube for Perforating Gun

 

 

 

 

 

 

Tube for Perforating Gun

 

 

 

 

 

 

 

 

 

 

 

 

 

 

1

60

2.36

60

90

45,60,90,120,180

2, 2.5,

3, 4,

7, 11,

15,21

2

68

2.68

68

85

3

73

2.87

73

105

4

80

3.15

80

105

5

89

3.50

88.9

105

6

102

4.00

101.6

105

7

114

4.50

114.3

105

8

118

4.65

118

105

9

127

5.00

127

90

10

127

5.00

127

105

11

178

7.00

177.8

90

12

42

1.65

42

140

13

51

2.01

51

140

14

73

2.87

73

140

15

 

 

 

83

3.27

83

140

16

86

3.37

85.7

140

17

89

3.50

88.9

140

 

 

18

102

4.00

101.6

140

19

127

5.00

127

140

20

Super-high pressure

89

3.50

88.9

175

60,90

21

121

4.76

121

175

60

22

reinforced ultra-high pressure

89S

3.50

88.9

210

60,90

Tube for Perforating Gun

 

 