SUS420F Seamless Stainless Steel Tube
Carbon (C): about 0.26-0.35%
Chromium (Cr): approx. 12-14 percent
Manganese (Mn): up to 1.0 percent
Silicon (Si): up to 1.0 percent
Sulphur (S): approx. 0.15-0.35 percent
Phosphorus (P): up to 0.04 percent
Machinability: SUS420F is a free-cutting stainless steel, and its sulphur content improves cutting performance, making it easy to cut and turn during machining.
Similar to other SUS420 series stainless steels, SUS420F may have relatively low corrosion resistance. This means that use in corrosive environments should be limited.
Applications: Due to its easy machinability, SUS420F is commonly used in applications requiring high mechanical properties and easy machinability, such as bolts, nuts, bearings and other mechanical parts. However, due to the limitations of its corrosion resistance, it may need to be carefully selected for applications used in corrosive environments.
| SUS420F | |
|
10m-12m,12m or as customer's actual reques. |
|
|
Transparent oil,anti-rust oil According to clients requirement |
|
|
Within 7 days, According to the quantity ordered by the customer. |

We have full stock, and products can be delivered within 14 days. Multiple styles for your choices.

1.Q: Are you a manufacturers and what is your production capacity?
2.Q: What product information do I need to provide?
3.Q: How do you guarantee the quality of your products?
Popularni tagovi: sus420f seamless stainless steel tube, China sus420f seamless stainless steel tube manufacturers, suppliers, factory, 2205 Dupleksna cijev od nehrđajućeg čelikaASTM A790 2205 Dupleks nehrđajući čelik bešavne cijeviSuper dupleks nehrđajući čelik bešavna cijevBešavna okrugla cijev od nehrđajućeg čelikaS31803 Dupleks cijev od nehrđajućeg čelika
Pošaljite upit